A Welding Procedure Specification is a written document that defines how a specific weld should be made. It specifies the variables a welder must follow — base material, filler material, process, preheat, interpass temperature, joint design, and more — to produce a weld that meets the required mechanical and quality properties.
A WPS is not optional in most industrial contexts. Standards such as ISO 15614, ASME Section IX, AWS D1.1, and EN ISO 15609 require qualified procedures before production welding begins. Without one, a fabricator cannot demonstrate that the weld was made under controlled, repeatable conditions.
What a WPS contains
Every WPS covers a defined set of variables. Essential variables are those where a change invalidates the existing qualification — switching base material group, filler material, or welding process, for example. Supplementary essential variables apply when impact testing is required. Nonessential variables can be adjusted within limits without requalification, though they must still be documented.
Typical content includes: welding process and transfer mode, base material specification and thickness range, filler material classification and diameter, joint configuration and preparation, position and travel direction, preheat and interpass temperature limits, post-weld heat treatment requirements, and shielding gas composition and flow rate.
Standards that govern WPS
The applicable standard depends on the industry and market. EN ISO 15614-1 covers arc and gas welding of steels and is the standard most used in European pressure equipment and structural work. ASME Section IX applies to pressure vessels and piping under US and many international codes. AWS D1.1 governs structural steel welding for buildings and bridges. Each standard defines its own essential variables, qualification ranges, and testing requirements — so the WPS must be written and qualified against the specific standard the project demands.
WPS and PQR: how they connect
A WPS must be supported by a Procedure Qualification Record. The PQR is the test evidence: a record of the actual welding parameters used on a test piece, together with the results of mechanical testing. The WPS draws its qualification range from the PQR — the ranges permitted by the applicable standard based on what the test piece demonstrated.
One PQR can support multiple WPSs, as long as the production variables fall within the qualified ranges. When parameters change beyond those ranges, a new PQR test is required before the WPS can be updated or a new one written.
Managing WPS across production
For companies with multiple active WPSs, tracking which procedure applies to which joint, ensuring welders have current revisions, and maintaining the link between WPS and PQR becomes a documentation challenge. Missing a revision, issuing an outdated WPS, or failing to produce the supporting PQR during an audit are common findings in fabrication quality audits.
Digital welding documentation systems address this by storing WPS and PQR together, linking them to specific jobs and weld joints, and making the current revision available to production personnel without manual distribution. See how SOCWeld structures welding documentation to keep WPS, PQR, and welder qualification records connected and audit-ready.
FAQ
What is the difference between a WPS and a PQR?
A WPS tells the welder how to make a weld. A PQR is the test record that proves the procedure produces acceptable mechanical properties. The WPS is qualified based on the PQR.
Does every weld need its own WPS?
Not necessarily. One WPS can cover a range of material thicknesses, joint types, and positions, as defined by the applicable standard. The goal is to cover production welds within a qualified range, not to write a separate WPS for every joint.
Who can approve a WPS?
Approval requirements vary by standard and contract. Some standards allow the manufacturer to approve their own WPS based on a qualified PQR. Others require a third-party inspection body. Check the specific standard and any customer or regulatory requirements before issuing a WPS.
What happens if production parameters deviate from the WPS?
Deviations from essential variables require a new qualification test. Deviations from nonessential variables may be allowed within limits but must be documented. Undocumented deviations are a non-conformance and can result in rejection or rework.
How long is a WPS valid?
A WPS itself does not expire, but the supporting PQR must remain on file. If the PQR is lost or the test evidence is questioned, the WPS loses its qualification basis. Some contracts or standards impose periodic review requirements.
Can I use a WPS from a subcontractor?
In some cases, yes — if the standard permits it and the subcontractor’s PQR supports the required qualification range. This needs to be agreed with the client and verified against the applicable standard before production starts.
Ready to move your WPS management off spreadsheets? Book a demo to see how SOCWeld handles procedure documentation in practice.